News

Liebherr LR1300 Track Shoe Mechanical Performance Test

Liebherr LR1300 Track shoe mechanical performance test

  Value Machinery Manufacture is a company that integrates production and sales with high quality standards. We mainly produce and sell Crawler Crane Undercarriage Parts, including: Top roller, Bottom roller, track shoe, Idler, Sprocket ,and so on. Our philosophy is based on product quality, supplemented by service quality, to ensure that every customer can Our company purchases good products and enjoys good service.

  We have a professional quality inspection department, they will strictly control the quality inspection of products during the production process.

 

  On Monday, the quality inspection department reported on the Machaical properties test of the Liebherr LR1300 track shoe that had just completed Quenching & Tenpering.

23-11

1. Tensile Strength

Tensile Strength is the critical value of the transition of metal from uniform plastic deformation to local concentrated plastic deformation, and it is also the maximum bearing capacity of metal under static tension conditions. Tensile strength is the resistance to the maximum uniform plastic deformation of the material. Before the tensile sample is subjected to the maximum tensile stress, the deformation is uniform, but after exceeding, the metal begins to shrink, that is, concentrated deformation; Very small) brittle material with uniform plastic deformation, which reflects the fracture resistance of the Liebherr LR1300 track shoe.

2. Yield Strength

Yield Strength is the yield limit when the metal material yields, that is, the stress that resists micro-plastic deformation. For metal materials without obvious yield, the stress value that produces 0.2% residual deformation is specified as its yield limit, which is called the conditional yield limit or yield strength. It mirrors the plasticity and toughness of the Liebherr LR1300 track shoe.

3. Impact Toughness

Impact Toughness refers to the ability of a material to absorb plastic deformation work and fracture work under impact loads, reflecting the internal micro-defects and impact resistance of the material. The actual significance of the Impact Toughness index is to reveal the brittle tendency of the material and to reflect the resistance of the metal material to external impact loads.

IMG3704

4. Elongation

Elongation refers to the percentage of the ratio of the total deformation ΔL of the gauge section after tensile fracture to the original gauge length L: δ=ΔL/L×100%.

  Cold-rolled steel strip after recrystallization annealing needs to be tempered to obtain various properties required for delivery. Elongation, as the only deformation index of temper rolling, plays a vital role in ensuring the performance of the internal structure of the strip.

1111

 

  Liebherr LR1300 track shoe did not disappoint us in the results of four aspects of mechanical performance testing, and continued to maintain excellent standards.

 